Alloy Steel grade 12.9? 3

Status
Not open for further replies.

mbfree

Mechanical
Nov 2, 2006
13
Hi,
I am looking for a composition information on what is referred to as "Alloy Steel, grade 12.9"

Any help would be appreciated....
 
Replies continue below

Recommended for you

Property Class 12.9 is for externally threaded fasteners. You can find the requirements in ISO 898-1 or ASTM F 568M.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 