I'm trying to design and build a next-gen heat exchanger that operates at 950 C and 70 Bar. Does anyone know what alloys I could use for this application? I know alloy 617 would work, but am having a hard time getting it.
 
Replies continue below

Recommended for you

sjewenp;
I'm trying to design and build a next-gen heat exchanger that operates at 950 C and 70 Bar. Does anyone know what alloys I could use for this application?


Yes, and you will have few choices. Start getting familar with ASME B&PV Code, Section VIII, Div 1 and Section II, Part D and Section IX.
 