Hi;
I have almost no experience with material finishes on metal. Our customer needs a finish of 125 microinches (or better) on Alloy 715. This is a 70-30 Copper-Nickel alloy. Does anyone know if that alloy can get that finish, and if so, by what method(s)? Finally, does anyone know any commercial shops that do a good job with this kind of request?
Thanks very much!
Ron
I have almost no experience with material finishes on metal. Our customer needs a finish of 125 microinches (or better) on Alloy 715. This is a 70-30 Copper-Nickel alloy. Does anyone know if that alloy can get that finish, and if so, by what method(s)? Finally, does anyone know any commercial shops that do a good job with this kind of request?