I have run a welding procedure test to ASME IX. Details:
2" sch 40 pipe butt weld with GTAW using an alloy 625 filler wire. 5G positon, max interpass 150°C
It has failed the tensile test: failure in weld metal - values 750 to 800 MPa.
The parent material Alloy 625 grade 2(SB-444) is specified with minimum UTS of 827MPa.
Speaking to the filler wire supplier they would expect a minimum of 730MPa.
Speaking to someone else, they have found alloy 625 all weld metal to have UTS < 800MPa.
Can anyone provide a solution to getting an alloy 625 procedure to pass?
Thanks
2" sch 40 pipe butt weld with GTAW using an alloy 625 filler wire. 5G positon, max interpass 150°C
It has failed the tensile test: failure in weld metal - values 750 to 800 MPa.
The parent material Alloy 625 grade 2(SB-444) is specified with minimum UTS of 827MPa.
Speaking to the filler wire supplier they would expect a minimum of 730MPa.
Speaking to someone else, they have found alloy 625 all weld metal to have UTS < 800MPa.
Can anyone provide a solution to getting an alloy 625 procedure to pass?
Thanks