May 4, 2010 #1 BigTank Mechanical Joined Sep 24, 2007 Messages 368 Location US I am not used to working with copper alloys. Why is it that C70600 is in the ASME Sect. II-D table Y-1, but the seemingly more common C44300 is not? -------------------------------- Fitter, happier, more productive
I am not used to working with copper alloys. Why is it that C70600 is in the ASME Sect. II-D table Y-1, but the seemingly more common C44300 is not? -------------------------------- Fitter, happier, more productive
May 6, 2010 #2 MrBTU Mechanical Joined Dec 3, 2009 Messages 104 Location US Big Tank - Excellent point. We have brought this up numerous times in the past with Code folks. We use 15ksi in our calcs. Upvote 0 Downvote
Big Tank - Excellent point. We have brought this up numerous times in the past with Code folks. We use 15ksi in our calcs.