Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Allowing Surfaces to Slip under Thermal Expansion

Status
Not open for further replies.

goldenspark

Electrical
Joined
Apr 22, 2004
Messages
6
Location
FR
We have a system that has a polished aluminium surface pressed onto a smooth copper coated ceramic one.
Because of differential thermal expansion the aluminium will spread radially and pull the ceramic into tension.
We think we need to have a low enough coefficient of friction between the two surfaces to allow them to slip before it fractures the ceramic, but are struggling to quantify it.
The problem is that the two materials are being compressed together at about 4 N/mm2 (600 psi) pressure, to doing full scale testing is impractical. Testing so far seems to be suggesting we need a lubricant (we have tried oil).
Is our only practical option to do small area testing, or are there any other options anyone can suggest?

We are wondering about Rhodium plating or similar dry system instead of a fluid lubricant, which would better suit other requirements.

On a related subject, would a test at a lower pressure be valid, or do real world effects such as asperity crushing make this invalid?
 