Hi there,

How are you doing today? Hoping that you feel very well.
I made a simulation of a fluid transfert pipe. All is doing well in my piping simulation with CAESAR II but I don't know how to compute the material's A333 6 allowable stresses.

How can we compute the allowable stresses? SC, sh1, Sh2, sh3, ....

Thank you for your help.

Best regards!
 
XL83NL,
Thank you for your answer, the allowable stresses for A333 6 are note avalable in the library or the CODETI Code
 
Is CODETI still supported? When Googling on CODETI Piping, there's no French site, such as an authority, still publishing this standard. Isn't it withdrawn already?

Huub
 
What design code are you working to?

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
OP mentioned CODETI, the former French national piping code, which I believe is based on B31.3.

Huub
 
These are from B31.3, First one is min temp, second min tensile (Mpa), Min yield and Max temp.

Next set are the allowable values from 40C up to 600 - 138 MPa up to 200C

image_dgvmni.png


image_luar8t.png


Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Thank you for your answers, I appreciate it.

My client demands to do the calculations using CODETI.
 
Go to snct.org and codeti 2010 divison 2 is what I think you're looking for.

But find someone who reads French.

And has deep pockets - the code seems to be listed at €2,700 !!!

Remember - More details = better answers