Jun 17, 2002 #1 Guest How do I calculate the allowable stress of ASTM A350 LF6 Class 2 Stainless Steel at 210 deg F?
Dec 10, 2002 #2 EORC Materials Joined May 20, 2002 Messages 1 Location HK you should check the data from ASME SEC II PART D allowable stress Upvote 0 Downvote
Jul 5, 2003 #3 arifpatel Mechanical Joined May 28, 2003 Messages 4 Location SA ASTM A 350 LF6 class 2 is carbon steel forging material. Check in ASME B31.3 Table 1 Upvote 0 Downvote