Physical Properties
Depending on the composition, some glass will melt at temperatures as low as 500° C (900° F); others melt only at 1,650° C (3,180° F). Tensile strength, normally between 2,745 and 5,500 N/sq cm (4,000 and 8,000 lbwt/sq in), can exceed 68,650 N/sq cm (100,000 lbwt/sq in) if the glass is specially treated. Specific gravity (density relative to water) ranges from 2 to 8, or from less than that of aluminium to more than that of steel. Similarly wide variations occur in optical and electrical properties
Glass does not have any plastic
range. Glass is very strong 5x10^6 lb/in^2 but actual glass products exhibit strengths 500 to 1000 times lower due to surface imperfections and stress concentrations.
Theoretical strength is around 1 million psi, which whiskers approach, while the bulk material is around 5000 psi due to flaws in the glass, which cracks.