Does anyone have information on allowable stress in a steel-steel pin lug combination?
 
Replies continue below

Recommended for you

Thanks so far, but i am actually looking for the pin/lug of hydraulic rods. More specifically: hardened steel surfaces in pendulum motions. I am dealing with a seizure problem and there is some argument on the allowable surface stress limits.
 