Looking into brazing Al alloy 5056 to Al 6061-T4. Melting point for Al 5056 is 1055F-1180F while the melting point for 6061 is 1080F-1205. For general brazing of Al 6061 to 6061, usually recommend BAlSi-4 filler metal with a brazing temperature range of 1080-1100F.
Having trouble finding information for parameters of brazing Al 5056 to Al 6061.
I am looking for information for filler metal and brazing temperature range for brazing Al 5056 to Al 6061.
Having alot of trouble finding information for the above inquiry.
Any suggestions?

Thank you in advance.
 