Hello ETips,
I looking for a reference, article, paper or other source that may list the endurance/SN/Fatigue curve for the listed material, any suggestions avail are appreciated.
 
Have you tried the ASM Handbook?
You may have to live with data for 4140 (or 4145).
Timken used to publish this data but I can't locate it off hand.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 