Mar 25, 2021 #1 FOM1 Mechanical Joined Feb 10, 2021 Messages 4 Location US Hello ETips, I looking for a reference, article, paper or other source that may list the endurance/SN/Fatigue curve for the listed material, any suggestions avail are appreciated.
Hello ETips, I looking for a reference, article, paper or other source that may list the endurance/SN/Fatigue curve for the listed material, any suggestions avail are appreciated.
Mar 25, 2021 #2 EdStainless Materials Joined May 20, 2004 Messages 16,351 Location Waukesha WI USA Have you tried the ASM Handbook? https://www.asminternational.org/documents/10192/1849770/06181G_Sample.pdfYou may have to live with data for 4140 (or 4145). Timken used to publish this data but I can't locate it off hand. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed Upvote 0 Downvote
Have you tried the ASM Handbook? https://www.asminternational.org/documents/10192/1849770/06181G_Sample.pdfYou may have to live with data for 4140 (or 4145). Timken used to publish this data but I can't locate it off hand. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed