AISI 4140 80K MYS 1

Status
Not open for further replies.

Ruslanag

Petroleum
Joined
Mar 22, 2015
Messages
1
Location
AE
What is the maximum temperature AISI 4140 80K MYS can withstand?
 
Well that's a wide open question.

The strength will derate as temperature increases. In general, staying 100F below the temper temperature will maintain strength unless extended times are seen. Take a look at the Holloman-Jaffe parameter and equate the temperature/time used for the temper heat treatment to the same Holloman-Jaffe value for a reduced temperature of interest. This would give you an estimate of the time required at that reduced temperature to have the same effect as the temper heat treatment.
 