Greetings,

I'm looking for mechanical properties of AISI 316L. I found some of them at MatWeb, but I miss the last ones :(

I'm looking for :
- tenacity
- shear and stress properties for torsion and bending
- fatigue properties
- cyclic loading properties
- stress at break

Many thanks for help.

Best regards,


Cyril Guichard
Mechanical Engineer Consultant
France
 
Replies continue below

Recommended for you

I think that stress at break is UTS. Like most other austenitics the fatigue properties are quite bad.

What do you mean by cyclic loading properties? Reversed bend? tension to compression cycles?

Tenacity?

Nick
I love materials science!
 