I've got a mill cert for 1045 steel with a 100 ksi yield, I'm trying to figure out what they've done to get that high a yield. I think they may have dual-certified a 1050 steel as 1045. The composition shows 0.080 NI, 0.090 V, and 0.020 MO. I didn't think these quantities of these elements were found in such a common steel.