I hope this information is interesting to somebody. These are the colors of the AISC Steel Construction Manual.
Historical Review of AISC Manual 1927 to 2017
Summary of All Printings of “AISC Manual of Steel Construction”
Date of Included
Date of Included AISC Code of
Edition & Printing Date AISC Specification Standard Practice
ASD Manuals
1st Ed., 1st Printing Dec. 1927 6-1-23 10-1-24 Black Book
1st Ed., 2nd Printing Mar. 1928 6-1-23 10-1-24
1st Ed., 3rd Printing May 1928 6-1-23 10-1-24
1st Ed., 4th Printing Dec. 1928 11-1-28 1928
1st Ed., 5th Printing Apr. 1929 11-1-28 1928
1st Ed., 6th Printing Jan. 1930 11-1-28 1928
1st Ed., 7th Printing Apr. 1930 11-1-28 1928
1st Ed., 8th Printing Dec. 1930 11-1-28 1928
1st Ed., 9th Printing Jan. 1932 11-1-28 1928
1st Ed., 10th Printing Oct. 1932 11-1-28 1928
2nd Ed., 1st Printing Jan. 1934 1-34 1-34
2nd Ed., 2nd Printing Jan. 1934 1-34 1-34
2nd Ed., 3rd Printing May 1936 1-34 1-34
2nd Ed., 4th Printing May 1936 1-34 1-34
3rd Ed., 1st Printing Oct. 1937 1-37 1-37
3rd Ed., 2nd Printing 1939 1-37 1-37
3rd Ed., 3rd Printing 1940 1-37 1-37
3rd Ed., 4th Printing 1941 1-37 1-37
4th Ed., 1st Printing 1941 7-41 7-41
4th Ed., 2nd Printing 1942 7-41 7-41
4th Ed., 3rd Printing 1943 7-41 7-41
4th Ed., 4th Printing 1944 7-41 7-41
4th Ed., 5th Printing 1945 7-41 7-41
5th Ed., 1st Printing 1946 2-46 11-1-45
5th Ed., 2nd Printing 1947 2-46 12-1-46
5th Ed., 3rd Printing 1947 2-46 12-1-46
5th Ed., 4th Printing 1947 2-46 12-1-46
5th Ed., 5th Printing 1948 2-46 12-1-46
5th Ed., 6th Printing 1948 2-46 12-1-46
5th Ed., 7th Printing 1948 2-46 12-1-46
5th Ed., 8th Printing 1949 2-46 12-1-46
5th Ed., 9th Printing 1949 2-46 12-1-46
5th Ed., 10th Printing 1950 6-23-49 12-1-46
5th Ed., 11th Printing 1951 6-23-49 12-1-46
5th Ed., 12th Printing 1951 6-23-49 12-1-46
5th Ed., 13th Printing. 1952 6-23-49 12-1-46
5th Ed., 14th Printing 1952 6-23-49 6-26-52
5th Ed., 15th Printing 1953 6-23-49 6-26-52
5th Ed., 16th Printing 1954 6-23-49 6-26-52
5th Ed., 17th Printing 1955 6-23-49 6-26-52
5th Ed., 18th Printing 1955 6-23-49 6-26-52
5th Ed., 19th Printing 1956 6-23-49 6-26-52
5th Ed., 20th Printing 1956 6-23-49 6-26-52
5th Ed., 21st Printing 1957 6-23-49 6-26-52
5th Ed., 22nd Printing 1957 6-23-49 6-26-52
5th Ed., 23rd Printing 1958 6-23-49 6-26-52
5th Ed., 24th Printing 1959 6-23-49 6-26-52
5th Ed., 25th Printing 1959 6-23-49 6-26-52
5th Ed., 26th Printing 1960 6-23-49 6-26-52
5th Ed., 27th Printing 1961 6-23-49 6-26-52
5th Ed., 28th Printing 1961 6-23-49 6-26-52
5th Ed., 29th Printing 1962 6-23-49 6-26-52
5th Ed., 30th Printing 1962 6-23-49 6-26-52
6th Ed., 1st Printing July 1963 4-17-63 2-20-63 Maroon Book
6th Ed., 2nd Printing Aug. 1963 4-17-63 2-20-63
6th Ed., 3rd Printing Dec. 1963 4-17-63 2-20-63
6th Ed., 4th Printing Mar. 1964 4-17-63 2-20-63
6th Ed., 1st Revised P. Apr. 1965 4-17-63 2-20-63
6th Ed., 2nd Revised P. Nov. 1965 4-17-63 2-20-63
6th Ed., 3rd Revised P. Mar. 1966 4-17-63 2-20-63
6th Ed., 4th Revised P. Mar. 1967 4-17-63 2-20-63
7th Ed., 1st Printing 1970 2-12-69 6-1-70 Light Blue Book
7th Ed., 1st Revised P. 1973 2-12-69 10-1-72
Supplement 1, 11-1-70
Supplement 2, 12-8-71
8th Ed., 1st Printing 1980 11-1-78 9-1-76 Red Book
Supplement 1, 3-11-86
Supplement 2, 1-1-89
8th Ed., 2nd thru 11th
Impressions 9-80 thru 4-84 Same as above 9-1-76
8th Ed., 1st Revised P. Nov. 1984 Same as above 9-1-76
8th Ed., 2nd Revised P. Sept. 1987 Same as above 9-1-76
8th Ed., 3rd Revised P. Mar. 1988 Same as above 9-1-76
9th Ed., 1st Printing July 1989 6-1-89 9-1-86 Green Book
9th Ed., 2nd Impression Sept. 1989 6-1-89 9-1-86
9th Ed., 3rd Impression Jan. 1990 6-1-89 9-1-86
9th Ed., 1st Revision Jan. 1991 6-1-89 9-1-86
9th Ed., 2nd Revision Nov. 1995 6-1-89 9-1-86
LRFD Manuals
1st Ed., 1st Printing Nov. 1986 9-1-86 9-1-86 Blue Book
Supplement 1, 1-1-89
2nd Ed., 1st Printing 1994 12-1-93 6-10-92 Silver Book
3rd Ed., 1st Printing Dark Blue Book
METRIC LRFD Manual
1st Ed., 1st Printing 1999 1-30-1998 Orange Book
Combined Manuals
13th Ed., 1st Printing Dec. 2005 Black Book
14th Ed., 1st Printing Mar. 2011 Maroon Book
15th Ed., 1st Printing 2017 XXXX Book
The basis of this information comes from a list I downloaded from the AISC website. From the start of the list up to, and including, the LRFD Manual 2nd Ed. is from the information I got from the AISC website. I have added from the LRFD 3rd Ed. to the 15th Ed. I know it is not complete but all errors are my responsibility.
Jim
Hope somebody finds this useful. I also hope Ingenuity doesn't consider this a hi-jack. I now have seen some of the advertisements for the 1st Ed. LRFD Manual with a Red cover instead of a Blue cover.