I'm looking at Airbus's SRM that states the seat track specification DAN2001T79511. Does anyone knows where I can find the conversion of DAN2001? is it equivalent to 7075?
 
Replies continue below

Recommended for you

The easiest and safest way is to get in touch with Airbus product support in Toulouse.
If necessary I can pm you the telephone number, but really if you’re working with Airbus aircraft you should have the number.
 
It's been a few years since I worked on an airbus, but I believe they had a standards manual or some kind of manual equivalent to it. I believe it was available via CDrom. When I get back into the office next week, I will see if I still have a copy and see if DAN2001 is listed.
 
hi sych.
Acc A340 SRM DAN2001 specification is QQ-A-200/11
But seat track material in Srm are made 7075T76511