I have seen that during placing of concreting using tremie in bored pile they are placing a air pipe or vent pipe in the hopper to allow the flow of air and i had also seen many times air coming out from the pipe,my doubt is how air struck inside the pile when it is full of bentonite solution ......
 
Replies continue below

Recommended for you

The tremie process puts air into the system at the interface with the bentonite slurry. It introduces air in "gulps" and has to "burp".
 
Take a drink of water....swallow large amounts several times in a row and see the result...
 