I have an air cooler for Hydrogen service with high pressure. It is specified that header be plug-box type, which is ok. But it is also specified that tube to tubesheet joint shall be strength welded.
Is this mechanically possible? If API 661 establish that PWHT shall be performed before tubing. Is it possible to make strength weld through the holes of the plug ??
Is there another way ???
Header with removal cover is not allowed because of the Hydrogen service…
I also wonder if the strength welding of the tube to tube sheet joint is really necessary.
Thanks for your help.
GH
Is this mechanically possible? If API 661 establish that PWHT shall be performed before tubing. Is it possible to make strength weld through the holes of the plug ??
Is there another way ???
Header with removal cover is not allowed because of the Hydrogen service…
I also wonder if the strength welding of the tube to tube sheet joint is really necessary.
Thanks for your help.