We have some extruded bar stock of PTFE that has been in storage inside, out of the sun, under fairly dry conditions for several decades. I don't think there are any aging issues, but I thought I should check. Does anyone have any data showing a shelf life for this material?
 
Replies continue below

Recommended for you

Various websites suggest that PTFE has unlimited shelf life in a benign environment:

TTFN
faq731-376
7ofakss

Need help writing a question or understanding a reply? forum1529
 
Stores forever, unlike in service.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
ptfe got unlimited shelf life .

UV properties need to considered when designing ..
 
Test it and see if there are any property changes.
 