In order to calculate the temps, an exhaust catalyst design engineer would need info like:
Engine size and RPM (flow)
Exhaust inlet temp;
Catalyst internal volume;
Catalyst formulation;
Catalyst construction (honeycomb, pellet, asymmetric grid);
Exhaust composition at inlet;
Catalyst efficiency target;
Air injection;
2 bed or 3 bed cat;
What fuel will be used?
As SBBlue stated, air fuel ratios;
One more thing, what have you done to determine the results? The weblink you provided does not work.