There has been some discussion here on aerodynamics, Cd, downforce, so here goes:
On the Lexus LS 430 there are wheel spoilers, (air dams?) located on the undercarriage in front of each wheel well. They are made of synthetic rubber, are about 200mm wide and extend about 30mm down from the car body. I assume the Lexus engineers put such things on cars for a reason. What is the design intent? More downforce? Less drag?
BTW, these Lexus LS 430s do not have dimpled panels on the undercarriage, they have corrugated plastic panels, each corrugation about one inch wide.
On the Lexus LS 430 there are wheel spoilers, (air dams?) located on the undercarriage in front of each wheel well. They are made of synthetic rubber, are about 200mm wide and extend about 30mm down from the car body. I assume the Lexus engineers put such things on cars for a reason. What is the design intent? More downforce? Less drag?
BTW, these Lexus LS 430s do not have dimpled panels on the undercarriage, they have corrugated plastic panels, each corrugation about one inch wide.