Personally I had never heard of the stuff until I started looking at building a workshop.

It has some brilliant properties, but admit the more I digged into it the more involved it was designing with it and onsite compliance with plans.

Locally to me builders really don't want to change their methods. Or materials used. The sites I have seen using it they all seem to use black bar reinforcement. Which is a huge no no. The architects also seem love to pour c20 to fill gaps which messes with the weight loading and gives dissimilar stress concentrations.

Code wise it's lumped in with general construction codes. Australia seems to have a sub set for it.

I have found you need to think of the stuff as a bath sponge. And you need to design round moisture transport, letting it breath and move. Here they cover the stuff with moisture barrier or some other form of barrier which stops evaporation off its surface. Then it just loads up with water. As it's 80% air it's no wonder things fail when it doubles in weight.
 
Replies continue below

Recommended for you

I am lucky in my region one of the local products is high quality glass so the local uncertified sand basically extremely high grade silca glass grade.

the locals just dig it out the ground and use it. i have only used certified concrete for the foundations. .

if i need buffer sand its phone call and then 5 tons turnup inside 2 hours. its glacial moraine sand and its just packing.

There is a radon issue with aerated but not with my local product.
 
on the subject of builders not looking at drawings.

This is some fisheries building in India.

Seems to be international completely ignoring the drawings

357703620_654967890008509_4691628551906859698_n_tsbrkr.jpg
 
I knew but it made me laugh and think of what we were talking about.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor