Hi
We have 2 power generation plants with 2 import/export Transformers 55MVA 11kV/66kV with on load tap changer.
We do not have any spare parts for the time being. We have some corrosion issue as we are near the sea.
Do you advise to buy some spare parts or a new transformer? Replace the more corrodded one. Then refurbished old transformer & keep as spare?
What spare parts do you recommend to buy? Thanks