Jul 30, 2014 #1 msten979 Geotechnical Joined Jul 30, 2014 Messages 2 Location CA I am trying to compile a list of adverse effects of using CIP piles in soil contaminated with hydrocarbons. Any input would be greatly appreciated!
I am trying to compile a list of adverse effects of using CIP piles in soil contaminated with hydrocarbons. Any input would be greatly appreciated!
Jul 30, 2014 #2 Ron Structural Joined Sep 24, 1999 Messages 16,336 Location US The strength gain of concrete can be severely affected by hydrocarbons. Upvote 0 Downvote