We are looking for an alternative to standard DOM tubing for a 4 link. And I was curious if anyone had any success with ADI for suspension systems? I've done a lot of research and I can only find an article on when Ford used for the 99 Mustang as well as some older info on rear ends. But nothing new.
If you have perhaps you can answer some items I am unsure about. Mainly I am concerned with the ductility of the material. Normally we would use a DOM tubing, which in itself is light weight, strong, tuff and ductile (elongation before break (15-20%). As well there is a substantial difference between the yield and tensile, which is sort of a rough indicator of the toughness.
While adi has 110 tensile, 75 yield and an elongation of 11%. As well the reduction of error is low around 10%. Based on these numbers it would not be as tough or ductile. But further research has shown this not to be the case. As impact and fracture strength are quite high.
The reason for the change is purely cosmetic, we need something nicer than a simple tube.
If you have perhaps you can answer some items I am unsure about. Mainly I am concerned with the ductility of the material. Normally we would use a DOM tubing, which in itself is light weight, strong, tuff and ductile (elongation before break (15-20%). As well there is a substantial difference between the yield and tensile, which is sort of a rough indicator of the toughness.
While adi has 110 tensile, 75 yield and an elongation of 11%. As well the reduction of error is low around 10%. Based on these numbers it would not be as tough or ductile. But further research has shown this not to be the case. As impact and fracture strength are quite high.
The reason for the change is purely cosmetic, we need something nicer than a simple tube.