Looking for an adhesive/clamp type splice to form an endless belt. Need low profile splice.
Belt: Urethane 7/8 pitch timing belt x 2" wide with 29 .0355" steel reforcing wires.
Belt breaking strength 6,000 lbs.
Currnetly stripping ends of urethane belt to expose wires and using pinned steel clamping hinge with 2 part epoxy adhesive (Hernon Fusion Bond #372F) to clamp wires in steel splice hinge.
Can achieve 75% strength.
Need help with prep procedure and epoxy application procedure. Any other suggestion would help.
Thanks
Belt: Urethane 7/8 pitch timing belt x 2" wide with 29 .0355" steel reforcing wires.
Belt breaking strength 6,000 lbs.
Currnetly stripping ends of urethane belt to expose wires and using pinned steel clamping hinge with 2 part epoxy adhesive (Hernon Fusion Bond #372F) to clamp wires in steel splice hinge.
Can achieve 75% strength.
Need help with prep procedure and epoxy application procedure. Any other suggestion would help.