I have some smooth rubber applied to aluminum on an outdoor application using 3M77 spray adhesive that isn't working.
The rubber heats up, expands and comes loose. I need something that's not permanent, but will handle the heat. The material gets to a temp whereby you can only keep your hands on it for about 3 seconds before real pain sets in, not sure what temp that is? 150F?
I plan on the 3M90 spray unless someone else can give me a hint of a commercially available material that I can buy at Home Depot type stores.
Double sided tape may be usable too but the 3M material I have is more permanent that I'd desire.
Thanks,
kch
The rubber heats up, expands and comes loose. I need something that's not permanent, but will handle the heat. The material gets to a temp whereby you can only keep your hands on it for about 3 seconds before real pain sets in, not sure what temp that is? 150F?
I plan on the 3M90 spray unless someone else can give me a hint of a commercially available material that I can buy at Home Depot type stores.
Double sided tape may be usable too but the 3M material I have is more permanent that I'd desire.
Thanks,
kch