Does anyone know of an adhesive that is compatible with hydrazine?
 
Replies continue below

Recommended for you

Well...what temperature, what exposure amount, and duration?

I assume you've looked at Eckhardt Schmidt's book. And here
Some epoxies may be okay for short term, room temp. or so - usually amine-cured epoxies do better than novolac resins. Short chain polyethylene might work, if you want a hot-melt, also at low temps.

This reference talks about an epoxy sealant modified to improve flexibility but maintain hydrazine resistance:
 