Dear Engineers
I have a quck question about additional wleding after PWHT
and Hydro test completely.
present situation is as follows.
In a vertical pressure vessel of ID3000mm, shell Thk 17mm
herewith, one of Internal supporter (T10mm x 50mm) was attached with 8mm fillet welding and then, this support was revomed as per client requirement.
In this condition, client ask for additional requirement as follows as per their precess requirement.
- PWHT again
- Hydrotest again.
However, this requirements is not related to ASME requirement, but only for process condition.
I have a quck question about additional wleding after PWHT
and Hydro test completely.
present situation is as follows.
In a vertical pressure vessel of ID3000mm, shell Thk 17mm
herewith, one of Internal supporter (T10mm x 50mm) was attached with 8mm fillet welding and then, this support was revomed as per client requirement.
In this condition, client ask for additional requirement as follows as per their precess requirement.
- PWHT again
- Hydrotest again.
However, this requirements is not related to ASME requirement, but only for process condition.