MatSci1254
Materials
Hi,
I have received A106 GR B seamless pipe for one of our project.
while checking the material test certificate of this pipes and relevant purchase specification I noticed that
- purchase spec specify Micro alloy steel shall not be used without prior approval.
- Nb and V contenet reported on MTC is 0.02% and 0.06%
- as per ASTM A106 Nb is non regulated elemenet( ASTM A106 does not specify limit for Nb) and mximum allowed content for v is 0.08%
My questions are
1) Does ASTM spec allow intentaionl addition of Micro alloy element?
2) How can we detrmine whether these elemenst are intentionaly added elements or are residual elements.
3) also does API 5L (for grade B and X42)allows intentional addition of micro ally elements
I have check ASTM A333 for GR 6 material, this spec does not allow delibrate addition of micro alloy element other those specified for Gr 6
Appreciate you advise.
I have received A106 GR B seamless pipe for one of our project.
while checking the material test certificate of this pipes and relevant purchase specification I noticed that
- purchase spec specify Micro alloy steel shall not be used without prior approval.
- Nb and V contenet reported on MTC is 0.02% and 0.06%
- as per ASTM A106 Nb is non regulated elemenet( ASTM A106 does not specify limit for Nb) and mximum allowed content for v is 0.08%
My questions are
1) Does ASTM spec allow intentaionl addition of Micro alloy element?
2) How can we detrmine whether these elemenst are intentionaly added elements or are residual elements.
3) also does API 5L (for grade B and X42)allows intentional addition of micro ally elements
I have check ASTM A333 for GR 6 material, this spec does not allow delibrate addition of micro alloy element other those specified for Gr 6
Appreciate you advise.