adding new oil to transformer

Status
Not open for further replies.

colonelbogart

Electrical
Jul 29, 2005
20
Dear all,

We have a leaking transformer and we are planning to repair it but since we need to fill more silicon oil can we just add any transformer silicon oil to existing?

Thank you.

Bogart
 
Replies continue below

Recommended for you

Yes, provided it meets the requirements for new silicone fluids in table 2 of C57.111. Just be careful not to mix silicone with mineral oil, or use any equipment for filling that was previously used with mineral oil. It will foam like an SOB.
 