Apr 10, 2006 #1 81671 Agricultural Joined Apr 10, 2006 Messages 5 Location DE Hello, I need to join CFC to metal. Does anybody know a brazing-alloy I can use? Thanks for all your answers!
Hello, I need to join CFC to metal. Does anybody know a brazing-alloy I can use? Thanks for all your answers!
Apr 10, 2006 #2 SWComposites Aerospace Joined Nov 6, 2000 Messages 3,722 Location US CFC = carbon fiber composite, chloro-floro-carbon, ??? What specific materials are you trying to join? Upvote 0 Downvote
CFC = carbon fiber composite, chloro-floro-carbon, ??? What specific materials are you trying to join?
Apr 10, 2006 #3 tomwalz Materials Joined May 29, 2002 Messages 947 Location US Contact Ron Smith at e-mail: solution@mri-bluebell.com http://www.materialsresources.com Thomas J. Walz Carbide Processors, Inc. http://www.carbideprocessor.com Upvote 0 Downvote
Contact Ron Smith at e-mail: solution@mri-bluebell.com http://www.materialsresources.com Thomas J. Walz Carbide Processors, Inc. http://www.carbideprocessor.com
Apr 10, 2006 Thread starter #4 81671 Agricultural Joined Apr 10, 2006 Messages 5 Location DE Hello Gentlemen, thanks you for your replys. I'm trying to join carbon fiber composites with metal...please excuse that I didn't write that clearly. Upvote 0 Downvote
Hello Gentlemen, thanks you for your replys. I'm trying to join carbon fiber composites with metal...please excuse that I didn't write that clearly.
Apr 10, 2006 Thread starter #5 81671 Agricultural Joined Apr 10, 2006 Messages 5 Location DE What may be important too, is that the CFC-part will be used in high temperatures (>1000°C)... Upvote 0 Downvote
Apr 11, 2006 #6 SWComposites Aerospace Joined Nov 6, 2000 Messages 3,722 Location US So what matrix material do you plan to use in the composite? tianium? inconel? ceramic? what metal are you joining to? 1000C is very hot! Upvote 0 Downvote
So what matrix material do you plan to use in the composite? tianium? inconel? ceramic? what metal are you joining to? 1000C is very hot!
Apr 11, 2006 Thread starter #7 81671 Agricultural Joined Apr 10, 2006 Messages 5 Location DE the matrix material will be carbon, the metal will inconel...what I want to know, is which brazing alloys I can use to wet the C/C... Upvote 0 Downvote
the matrix material will be carbon, the metal will inconel...what I want to know, is which brazing alloys I can use to wet the C/C...
Apr 12, 2006 #8 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US Why do you want to have a liquid metal contact your composite? Why not use a liquid polymeric adhesive? Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote
Why do you want to have a liquid metal contact your composite? Why not use a liquid polymeric adhesive? Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
Apr 12, 2006 Thread starter #9 81671 Agricultural Joined Apr 10, 2006 Messages 5 Location DE because of the high temperatures the compound will be used in... Upvote 0 Downvote