We have a linear actuator manufactured in China. We recently have been getting many failures at a stress concentration area of the screw.
The basic design is a 0.75" ACME screw. Threads machined off to a diameter of 12mm (.472"
where a 5mm (.197"
hole is drilled. A pin through this hole transfers the geared motor load and absorbs the thrust load. Our units are rated for a maximum load of 1000lbs. I have worked the max tortional load (lifting) to be 112 in.lbs. The screw has been breaking in half at the pin location. Material for the screw is 1015 and for the pin is SUM22 (apperantly the same as AISI 1213). RPMs are low (approx. 30rpm) Using the max shear theary I come up with 9763 psi shear load for the screw and 18131psi for the pin. I am not sure what the stress concentration factor should be for the tension load of the screw? The failures seam to be fatigue failure. Failures are occuring in the field at loads of 400lbs.
Any suggestions as to how to reduce failures without any major changes to the parts?
Do my stress analysis values seem right?
The screws are manufactured at the plant (threads are rolled). Therefore it is cold worked then the cold rolled thread is machined off. Should the new machined surface be cold rolled again?
What fraction of the yield strength should my max allowable stress be?
Will going to a higher carbon steel make the material more brital, thus more susceptible to failure?
Please help. Let me know if you need more info, I can provide it.
Thanks,
Beatcan
The basic design is a 0.75" ACME screw. Threads machined off to a diameter of 12mm (.472"


Any suggestions as to how to reduce failures without any major changes to the parts?
Do my stress analysis values seem right?
The screws are manufactured at the plant (threads are rolled). Therefore it is cold worked then the cold rolled thread is machined off. Should the new machined surface be cold rolled again?
What fraction of the yield strength should my max allowable stress be?
Will going to a higher carbon steel make the material more brital, thus more susceptible to failure?
Please help. Let me know if you need more info, I can provide it.
Thanks,
Beatcan