Acid Cleaning of 410SS

Status
Not open for further replies.

MirjafariSM

Mechanical
Feb 15, 2009
23
Hi all
i have a question.
as u know for A.S.S. generally acid cleaning done for degreasing and etc.
some of my vendors tell me that for 410ss, mechanical cleaning is better and they don't suggest acid cleaning for this type of steel.
are they true?
what is the reason?
best regards
 
Replies continue below

Recommended for you

sometimes the acid-bath can turn on you and start eating up your metal with martensitic stainless, esp. if you occasionally produce some nefarious microstructures, Cr-depleted areas; or if vendor process control is weak.
 