Do Acetone reacts with carbon steel to for mesityloxide? When we switch our storage tanks after few days, mesityloxide content will be high and gradually reduces when diluted with recovered acetone from columns.
Have you guys experienced this poblem before? If yes is there nay kind of inert coating you applied for carbon steel tanks?
Koshy
Have you guys experienced this poblem before? If yes is there nay kind of inert coating you applied for carbon steel tanks?