Feb 26, 2024 #1 kremenco Mechanical Joined Feb 24, 2005 Messages 24 Location AU Hi All, As per 2011 addenda of Div-2, the following detial 4.2.10.8 is not readily radiographable. However, in recent editions of Div-2 , it (Detail 4.2.10.7) is readily radiographable. What could be the reason for the change? Regards,
Hi All, As per 2011 addenda of Div-2, the following detial 4.2.10.8 is not readily radiographable. However, in recent editions of Div-2 , it (Detail 4.2.10.7) is readily radiographable. What could be the reason for the change? Regards,
Feb 27, 2024 1 #2 jt1234 Mechanical Joined Nov 17, 2022 Messages 107 Location US 45deg max vs. 45 deg min. Upvote 0 Downvote