Hercules28
Materials
Dear all,
I have some issues with some cast iron parts that are submersed in water. The water comes from a treatment facility but upon water testing I found high levels of chlorides in the range of 72mg/L.
I also have
Calcium 120mg/L
Fe 8 mg/L
Mg 12mg/L
Si 14mg/L
Na 28mg/L
Water is flowing...don't know the speeds. Any ideas? The part end corroded like 1/4 inch in 2 months.
I have some issues with some cast iron parts that are submersed in water. The water comes from a treatment facility but upon water testing I found high levels of chlorides in the range of 72mg/L.
I also have
Calcium 120mg/L
Fe 8 mg/L
Mg 12mg/L
Si 14mg/L
Na 28mg/L
Water is flowing...don't know the speeds. Any ideas? The part end corroded like 1/4 inch in 2 months.