Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

AC paving

Status
Not open for further replies.

cm61

Civil/Environmental
Joined
Mar 15, 2007
Messages
1
Location
US
I have a simple question, how many cubic yards are in a ton of Asphalt concrete paving ?
 
All of my sources for AC have a different weight. The weight veries from 2.04 to 2.10 tons per cubic yard of AC compacted to proper density.
 
I have 3774 lb/cy, or 1.89 tons, as delivered (uncompacted). But, it is in a spreadsheet, and I don't remember where I got that. I have used it many times for estimating in the past, and never had a bust in my calcs, though.

Engineering is the practice of the art of science - Steve
 
I've always used .057 T/SY per inch of depth, in place, for general estimating purposes. Which is about 2.04 T/CY compacted.
 
It varies with the density of your aggregate. I figure 2.0 to 2.2 ton/CY depending on the source.
 