AC Frequency

Status
Not open for further replies.

megbers

Mechanical
Joined
Feb 8, 2007
Messages
7
Location
US
How would one increase the frequency of an AC signal? I am looking into inductive heat treating and to my surprise the units are 10k dollars and up. I am trying to go from 110v, 60 hz to 110v, ~10kHz. Any ideas? Thanks
 
Possibly, an audio amplifier driven from a function (sine wave) generator. Higher power is available in guitar amplifiers.
 
I would think RF would be a problem if you did that. Heat trace cable has no need to be shielded at this point, so I doubt it is available.
 
I built something like this for my university thesis, except mine was a current-source inverter fed on a diet of 415V 3 phase at 20kW and an ample supply of cooling water.

How much power are you trying to transfer into the load? Audio amps for the semi-pro market are readily available up to about 1kW into a small load. A coupling transformer might be needed to impedance match the load coil to the amplifier. They're fun to build, especially trying to get hold of small quantities of large section ferrites.


----------------------------------
image.php

Sometimes I wake up Grumpy.
Other times I just let her sleep!
 
I've just watched the youtube clip. That is disturbingly similar to the thing I built, but a lot smaller. The highlight of my project was getting over 7000 people evacuated from the engineering buildings one snowy November day - my birthday funnily enough - after smoke started pouring out of a cable duct. There was a big inquiry about why the breakers had not tripped but I wasn't privy to any of that.
 
Very helpful info guys, thanks! Im looking to heat a ~1" dia steel rod to only about 400 deg on the surface. I dont think i need alot of power.
 
Ok, so the question is are you trying to achieve surface heating only or bulk heating? 10kHz suggests surface only in which case you need a powerful source to get energy into the surface layers faster than conduction can get it away from the surface into the core of the metal. Is this for a surface hardening application where you need a hard surface over a softer core? Also do you mean 400C or 400F? Big difference in power! I assume 400C for a metal hardening application.

BTW, have you considered adapting a bearing heater?

'Smoked,

My project was notorious enough before this incident: setting the university on fire elevated me to demigod status.


----------------------------------
image.php

Sometimes I wake up Grumpy.
Other times I just let her sleep!
 
You are not alone Scotty!

There is a commissioning engineer at ABB. He is named Smokey after he burned down a paper mill in Israel. He is also quite famous.

Gunnar Englund
--------------------------------------
100 % recycled posting: Electrons, ideas, finger-tips have been used over and over again...
 