I`m looking for the main global manufacturers/brands of sheet abs/polycarbonate sheet that:

is vac formable
available in vibrant colors (dont want to paint)
High gloss finish
uv/impact/scratch resisistant

Who are the major producers of plastic sheet (apart from GE plastics)?

ps its for a new luggage case and material will be sourced in south east asia.

Any help Appreciated
 
Replies continue below

Recommended for you

Have you tried google

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Yes Obviously! but was relying on people who have experiance in plastics and suppliers - hence asking the question
 
Bayer MaterialScience produces this type of product.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Thanks cory. Looked on website and they seem to offer a good alternative to GE plastics - will contact them.

If anybody else knows any other major producers of plastic sheet then let me know.

Thanks
 
Have you looked into Kydex? Sounds like it would meet your requirements, although I have no idea what your cost sensitivity is.
 