Gents,
I am looking for a material that has the best abrasive wear risistance for pump casing. it is horizantal duble suction volute pump for benzene service. the stream has solid particles and causing the casing/impeller to errod due to abrassive wear. Any idea where can i find a refernce for such application
upm
 
Typical abrasive resistant pump casings are cast from high chromium white iron, e.g. for slurry service. Another possibility is to refurbish your worn case with ceramic or possibly a benzene resistant urethane or rubber like material. I am assuming that the solids are relatively small particles. Operating conditions (pressure, temperature etc) will be a factor in your decision.
 
As suggested you could consider high chrome white iron or Ni Hard as abrasive resistant materials. If in case the solids are small you could also consider 17-4 PH or CA6NM materials.
 