Gents,
I am looking for a material that has the best abrasive wear risistance for pump casing. it is horizantal duble suction volute pump for benzene service. the stream has solid particles and causing the casing/impeller to errod due to abrassive wear. Any idea where can i find a refernce for such application
upm
I am looking for a material that has the best abrasive wear risistance for pump casing. it is horizantal duble suction volute pump for benzene service. the stream has solid particles and causing the casing/impeller to errod due to abrassive wear. Any idea where can i find a refernce for such application
upm