epoxy,
I just joined the Forum so I might be late for your request.
....however, you can run offset (in time) multifeeler caliper logs to determine the erosion progression and predict the lifespan of your pipe. Try to contact Kinley Corporation in Houston. They developed and running this type of survey for the last 50 years.
Good luck, Zax ;-)