tanvir.ce12
Civil/Environmental
Hi,
Some cylider specimen (4"x8") were casted & send them for compressive strength test after 14 days. I've used a nominal mix ratio of 1:1.5:3 for M20 grade concrete. But after crushing the strength of the three specimen is around 10.5ksi which is way higher than the target strength. What could be the reason behind that?
Some cylider specimen (4"x8") were casted & send them for compressive strength test after 14 days. I've used a nominal mix ratio of 1:1.5:3 for M20 grade concrete. But after crushing the strength of the three specimen is around 10.5ksi which is way higher than the target strength. What could be the reason behind that?