Hi Friends.
I have caterpillar 3516G gas engines 900kw, with ABB sace motorised ACB. Recently i m facing problem of its motor gear breakage. Generators are only 3 years old. Its a plastic gear mounted in side the motor unit and we had to replace complete motor assembly due this small grar. the broken gear looks to be very brittle and broke into pieces. If any one have the same expierience so that i would be in better positon to deal with ABB. Thanks for any response.
I have caterpillar 3516G gas engines 900kw, with ABB sace motorised ACB. Recently i m facing problem of its motor gear breakage. Generators are only 3 years old. Its a plastic gear mounted in side the motor unit and we had to replace complete motor assembly due this small grar. the broken gear looks to be very brittle and broke into pieces. If any one have the same expierience so that i would be in better positon to deal with ABB. Thanks for any response.