Hello,
I have a part meshed and solved for residual stresses.
I d like to delete a layer of mesh to simulate material removal but keep the remaining residual stress values.
What should i do step by step?
Thanks in advance.
 
Replies continue below

Recommended for you

You can remove elements with *Model Change, but you cannot enforce that the stresses stay the same. That depends on the situation (your boundary conditions, i.e.) and is calculated by the solver.
 
Actually, I don't want to enforce stresses stay the same.
What i want is to get what remaining residual stresses are after material removal.
I will use that phase of the mesh with pretension applied and material removed for new loading conditions.
Thanks.
 
No this is not like eroding plate or chip removal problem.
Yes i want to simulate chip removed (like machined) by using mesh layer (same size with removed chip) deleted and get the remaining stress state.
 
Sorry but you're not making much sense.

It is not a chip removal problem but it is?
 
As you know, there is tool chip removal problems solved. These are damage problems and i dont want to solve that problem as a damage one. I will try *Model change to deactivate some layers of mesh for the next loading step. I hope it will be satisfactory.
Thanks for your interest.
 