Hello, everyone!
I recently have downloaded Abaqus AM Modeler plugin and I was trying to go through workshop named "LDED_ThinWall". Everything was OK until I got some embarrassing results of the simulation. Maybe somebody could help me to figure out is it a modeling mistake, plugin bug or just my inattentiveness?
So the problem description:
It is a simulation of thin-wall tube which is printing by Laser Direct Energy Deposition method with material deposition and laser-path event series included in the model. After successful completion of two sequential jobs I was checking thermal and structural results and I saw that one wall doesn't get heat at all, it stays with initial temperature of 300 K, so it has most displacement and stresses.
The question is: what's wrong with workshop model or where should I make changes to make temperature distribution more uniform among all walls?
Please see attached image with results.
I recently have downloaded Abaqus AM Modeler plugin and I was trying to go through workshop named "LDED_ThinWall". Everything was OK until I got some embarrassing results of the simulation. Maybe somebody could help me to figure out is it a modeling mistake, plugin bug or just my inattentiveness?
So the problem description:
It is a simulation of thin-wall tube which is printing by Laser Direct Energy Deposition method with material deposition and laser-path event series included in the model. After successful completion of two sequential jobs I was checking thermal and structural results and I saw that one wall doesn't get heat at all, it stays with initial temperature of 300 K, so it has most displacement and stresses.
The question is: what's wrong with workshop model or where should I make changes to make temperature distribution more uniform among all walls?
Please see attached image with results.