A582 - S41600 Cond T / Mechanical Properties

Status
Not open for further replies.

EngineerRed

Mechanical
Joined
Jan 19, 2021
Messages
14
Location
IN
I'm looking for an authentic source for the mechanical properties of S41600 Cond T , I couldn't find them in ASME B&PVC Section II d , and in ASTM A582 either . Where else can I get this information ?
 
It won't be in the Code because it isn't an approved material.
The tensile properties should be just lime 410 as long as the C is the same.
You do need to know the exact C levels.
There are mill data sheets that have data for various tempers.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 